    • 摘要: 利用提拉法缓冷工艺,生长出掺Cr3+/离子的Li2GeO3晶体,按Tanabe-Sugano能级图和吸收光谱,计算出Cr3+在Li2GeO3晶体场中的光谱参数(Racach参数)为B=573 cm-1,C=2292 cm-1,Dq/B=23.八面晶场分裂参数:Δo=12 779 cm-1,在红外和近红外区激发Li2GeO3:Cr3+晶体,在796.2 nm,932.9 nm和962.5 nm处观测到有红外宽带发射。通过分析250 nm激发的荧光光谱,判断晶体中可能有Cr4+占据八面体心或八面体空位而引起在408.5 nm处的可见发射。

       

      Abstract: The Cr3+-doped Li2GeO3 crystal was grown by the Czochraski technique.The spectrum parameters of Cr3+. ions, Racah Coefficient, in Li2GeO3 crystal field were worked out:B=573 cm-1, C=2292 cm-1 Dq/B=2.23, Δo=12779 cm-1 and the split cofficient of octahed crystal field according to Tanabe-Sugano energy level diagram and the absorption spectra. The wide infrared emission bands in 796.2 nm, 932.9 nm and 962.5 nm region were observed. The visible emission excited with 250 nm light beam in 408.5 nm may be produced by Cr4+ in octahedral center.

       

    /